Linear Mold Shrinkage, Transverse 0.0063 - 0.0083 cm/cm

@Time 86400 sec
0.0063 - 0.0083 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP GX07409H PSU
LNP* LUBRICOMP* GX07409H is a compound based on PSU resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Healthcare.
Linear Mold Shrinkage, Transverse 0.0063 - 0.0083 cm/cm

@Time 86400 sec
0.0063 - 0.0083 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp GX07409X PSU
Wear resistant PSUThis data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0081 - 0.0083 cm/cm

@Time 86400 sec
0.0081 - 0.0083 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
Linear Mold Shrinkage, Transverse 0.0081 - 0.0083 cm/cm

@Time 86400 sec
0.0081 - 0.0083 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6