Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM-D1204 |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 18 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM-D1204 |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM-D1204 |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 25 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM-D1204 |
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 18 µm) HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66 PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.022 cm/cm @Thickness 3.20 mm |
0.018 - 0.022 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1733-GY1 Lubricated, Nucleated, Unfilled Nylon 6 Description: Lubricated, Nucleated, Unfilled Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® CE2055 NC010 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Perf.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Clariant Renol CP-MF-9 Acetal Copolymer Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |