Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0112 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0112 cm/cm
0.0112 in/in
STN 64 0808
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
Linear Mold Shrinkage, Transverse 0.0112 cm/cm
0.0112 in/in
Plastcom SLOVAMID 6 GF 7 T 13 PA6, 7% glass fibre, 13% mineral filling
FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli..
Linear Mold Shrinkage, Transverse 0.0112 cm/cm
0.0112 in/in
STN EN ISO 294-4
Plastcom SLOVAMID® 6 GF 25 FRC 4 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 25 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability according to UL 94 3 at 1,6mm, glow wire at 960°C. Applic..
Linear Mold Shrinkage, Transverse 0.0112 cm/cm
0.0112 in/in
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Linear Mold Shrinkage, Transverse 0.0112 cm/cm

@Thickness 2.00 mm
0.0112 in/in

@Thickness 0.0787 in
TPE Method
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric..
Linear Mold Shrinkage, Transverse 0.0112 cm/cm
0.0112 in/in
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY
Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America..
Linear Mold Shrinkage, Transverse 0.0112 cm/cm
0.0112 in/in
STN 64 0808
Plastcom SLOVAMID 66/6 GF 30 Polyamide 66/6, 30% Glass Fiber  (discontinued **)
FeaturesChemically reinforced alloy PA 66 and PA 6 with 30% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and el..
Copyright © lookpolymers.com All Rights Reserved