Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0081 cm/cm | 0.0081 in/in | |
Plastcom SLOVAMID 6 GF 20 FRG 3 PA6, 20% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 20 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 9.. |
|||
Linear Mold Shrinkage, Transverse | 0.0081 cm/cm | 0.0081 in/in | 60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Linear Mold Shrinkage, Transverse | 0.0081 cm/cm | 0.0081 in/in | 150x105x3; 280°C / MT 80°C; 500 bar; ISO 2577 |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0081 - 0.0083 cm/cm @Time 86400 sec |
0.0081 - 0.0083 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6 LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity. |
|||
Linear Mold Shrinkage, Transverse | 0.0081 - 0.0083 cm/cm @Time 86400 sec |
0.0081 - 0.0083 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6 4.0 specific gravity, Nylon 6 |
|||
Linear Mold Shrinkage, Transverse | 0.0081 cm/cm @Time 86400 sec |
0.0081 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MV005SX0 PP (Europe-Africa-Middle East) LNP* VERTON* MV005SX0 is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized. |