Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm | 0.0038 in/in | SABIC Method |
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific) CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa.. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP PDX-U-05314 PPA (Asia Pacific) LNP* Lubricomp* PDX-U-05314 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 - 0.0045 cm/cm @Time 86400 sec |
0.0038 - 0.0045 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EX08318C PEI (Asia Pacific) LNP* Stat-Kon* EX08318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm | 0.0038 in/in | ISO 294-4 |
Barlog Plastics KEBAFLOW MF130 LCP, 30% glass fiber reinforced LCP-GF30Information provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm | 0.0038 in/in | |
Plastcom SLOVALEN PH 49 GF 60 PP reinforced with 60% glass fibre Features: Modified homopolymer PP for injection moulding, chemically reinforced with 60% glass fibre, contains the modifier of mechanical properties.Very good strength and tensile modulus. Delivered.. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm | 0.0038 in/in | ASTM D955 |
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer
(discontinued **) XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe.. |