Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2600 cP @Temperature 25.0 °C |
2600 cP @Temperature 77.0 °F |
Mixed |
Lord Adhesives Circalokâ„¢ 6009 A/B Flame Retardant Epoxy Encapsulant Circalokâ„¢ 6009 A/B is a two component epoxy resin system which has moderate thermal conductivity and low viscosity. Circalokâ„¢ 6009 A/B meets UL 94V-0 specification for flame retardance.All.. |
|||
Viscosity | 2600 cP @Temperature 60.0 °C |
2600 cP @Temperature 140 °F |
|
BASF Pluracol® SG-470 Rigid Polyol Description: Pluracol® SG-470 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent .. |
|||
Viscosity | 2600 cP @Temperature 60.0 °C |
2600 cP @Temperature 140 °F |
|
BASF Pluracol® SG-450 Rigid Polyol Description: Pluracol® SG-450 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent .. |