Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ExxonMobil Mobil 1 0W-20 Mobil 1 W-20, Power and Performance Formula, is the most advanced performance synthetic engine oil designed to provide the ultimate level of power, and protection to keep engines running smoothly an.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | |
ChevronTexaco 68 AW Hydraulic Oil Texaco AW Hydraulic Oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants in high pressure service.Rust and corrosion protection — Gives excel.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | See Note 3. |
ChevronTexaco 904 Grease NLGI Grade 1/2 Texaco 904 Grease is a calcium soap grease. It contains graphite which enhances its lubricity.Typical test data are average values only. Minor variations which do not affect product performance are .. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ChevronTexaco ISO 68 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ChevronTexaco ISO 68 Hydraulic Oil AW FeaturesChevron Hydraulic Oils AW are designed to give excellent hydraulic pump protection. They are formulated with refined paraffinic base oils. They provide excellent antiwear protection, oxidati.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ChevronTexaco ISO 68 Ultra Gear Lubricant FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ChevronTexaco ISO 68 Utility Oil HVI FeaturesChevron Utility Oil HVI is a high quality, high viscosity index uncompounded oil with excellent water separating characteristics.Chevron Utility Oil HVI possesses good natural thermal and ox.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ChevronTexaco MERCON® V Automatic Transmission Fluid Beginning with the 1997 model year, Ford introduced a higher performance level ATF with the MERCON V specification. Many Ford automatic transmissions from 1999 on will require a MERCON V fluid. The .. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | |
ChevronTexaco Rando® HD 68 Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ChevronTexaco Regal® 68 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ChevronTexaco Rykon® ISO 68 Oil AW FeaturesChevron Rykon Oils AW are designed to give maximum hydraulic pump protection.Chevron Rykon Oils AW are formulated with ISOSYN® base stocks.They provide excellent antiwear protection, oxidat.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | |
ChevronTexaco Canopus® 68 Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant .. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | |
ChevronTexaco Havoline® MERCON® V Automatic Transmission Fluid Havoline Automatic Transmission Fluid MERCON V delivers value through:Protection against the formation of lacquers, sludge, or other harmful deposits.Exceptional stability provided by excellent base.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.4 cSt | 8.4 cSt | ASTM D445 |
ExxonMobil Mobil 1 0W-20 Mobil 1 W-20, Power and Performance Formula, is the most advanced performance synthetic engine oil designed to provide the ultimate level of power, and protection to keep engines running smoothly an.. |