Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco ISO 68 AIO

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco ISO 68 AIO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring antiwear or extreme pressure protection.They pass the Fresh Water Corrosion Test (ASTM D 665, Procedure A), and the severe Synthetic Sea Water Test (ASTM D 665, Procedure B). The natural thermal and oxidation stability of these lubricants, due to their high level of refinement, has been further enhanced by their unique additive systems. The high thermal and oxidation stability also reduces the possibility of oxidation deposits or the generation of acidic material from oxidation. Chevron AIO are able to withstand relatively high temperature operations for extended periods of time. They have very good demulsibility characteristics allowing quick release of moisture.They minimize entrained air which otherwise could result in low lubricant film strength between moving parts and pump cavitation.ApplicationsChevron AIO ISO 22 through ISO 150 are recommended for use in electric motor bearings, air compressors, gears, hydroelectric turbines, steam turbines, combustion turbine generators (gas), marine turbines, and hydraulic systems (except heavy duty systems, where Chevron Hydraulic Oils AW are recommended).These products can also be used as a general purpose ,machine oil for shop use. Their multifunctional characteristics allow them to replace other special application lubricants, resulting in reduced inventory and operating cost.
Physical Properties Metric English Comments
API Gravity 31.2 °
31.2 °
Viscosity Measurement 99
99
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 335 SUS
335 SUS
Saybolt Viscosity at 210°F 54.5 SUS
54.5 SUS
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 8.4 cSt
8.4 cSt
ASTM D445
Oxidative Stability >= 15.83 hour
>= 15.83 hour
25 psi pressure drop; ASTM D2272
>= 6000 hour
>= 6000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
Thermal Properties Metric English Comments
Pour Point -27.0 °C
-16.6 °F
ASTM D97
Flash Point 245 °C
473 °F
ASTM D92
Descriptive Properties Value Comments
Rust preventative Test Procedure B Pass
Synthetic Sea Water
Rust Procedure A, Distilled Water Pass
Users viewing this material also viewed the following: