Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Rykon® ISO 68 Oil AW

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Rykon® ISO 68 Oil AW.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Rykon Oils AW are designed to give maximum hydraulic pump protection.Chevron Rykon Oils AW are formulated with ISOSYN® base stocks.They provide excellent antiwear protection, oxidation and corrosion inhibition, as well as foam and aeration suppression.All grades have excellent demulsibility characteristics. Hydraulic systems, due to the nature of their operation, experience accelerated wear unless they are protected by clean, high quality antiwear hydraulic oils.Surging pressures in pumps and valves can increase metal-to-metal contact unless antiwear protection is present. The antiwear additives in Chevron Rykon Oils AW create a protective film on the metal surfaces. This protective film minimizes metalto-metal contact, which is most severe in vane- and gear-type pumps. As hydraulic pressures increase over 1000 psi, the need for antiwear protection increases proportionally.ApplicationsChevron Rykon Oils AW are most commonly used for hydraulics with vane- or gear-type pumps, especially where pressures exceed 1000 psi. They can also be used to lubricate lightly loaded reciprocating compressors and as general purpose shop lubricants for motors and bearings.Chevron Rykon Oils AW meet AGMA Specification 1 (ISO 46) and Specification 2 (ISO 68).Chevron Rykon Oils AW are registered with NSF International and are acceptable as a lubricant where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.
Physical Properties Metric English Comments
API Gravity 31.6 °
31.6 °
Viscosity Measurement 99
99
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 335 SUS
335 SUS
Saybolt Viscosity at 210°F 54 SUS
54 SUS
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 8.4 cSt
8.4 cSt
ASTM D445
Oxidative Stability >= 6000 hour
>= 6000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
ASTM D97
Flash Point 235 °C
455 °F
ASTM D92
Copyright © lookpolymers.com All Rights Reserved