Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 23 cSt | 23 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8310 (472) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 23 cSt | 23 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8311 (833-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 23 cSt | 23 cSt | Base Oil; ASTM D445 |
Nye Lubricants 833Z-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 23 cSt | 23 cSt | |
ConocoPhillips MV22 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Kinematic Viscosity at 40°C (104°F) | 23 cSt | 23 cSt | |
Lubriplate MAG-00 Lithium-Polymer Type Grease For Special Applications / Conditions These multi-purpose, lithium polymer greases have a wide operating temperature range for a variety of applications from -60°F to 300°F. Applications: Centralized systems, leaking gearboxes. MAG-00.. |
|||
Kinematic Viscosity at 40°C (104°F) | 23 cSt | 23 cSt | |
Lubriplate MAG-1 Lithium-Polymer Type Grease For Special Applications / Conditions These multi-purpose, lithium polymer greases have a wide operating temperature range for a variety of applications from -60°F to 300°F. Applications: Cold and wide temp. range, multi-purpose.MAG-1.. |