Lubriplate MAG-1 Lithium-Polymer Type Grease For Special Applications / Conditions

Category Fluid , Lubricant , Lithium Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate MAG-1 Lithium-Polymer Type Grease For Special Applications / Conditions.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
These multi-purpose, lithium polymer greases have a wide operating temperature range for a variety of applications from -60°F to 300°F. Applications: Cold and wide temp. range, multi-purpose.MAG-1 is available in Cartridges, Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 120 SUS
120 SUS
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 310
310
Unknown Amount of Work
Penetration P(60), 1/10 mm 340
340
Unknown Amount of Work
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Approx. Cold test
Dropping Point 191 °C
375 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 1
Rust/Oxidative Additives YES
Water Resistant YES