Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina E 911D40/77-IS Green PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | NBR NM-IEC 60811-1-3 |
Karina E TR-652D48/1-B-IS Black PVC Compound PVC Compound with NBR; recommended for injection of automotive parts and extrusion of flexible jacket for electrical cables.Information provided by Karina Indústria e Comércio de Plásticos .. |
|||
Specific Gravity | 1.27 - 1.29 g/cc | 1.27 - 1.29 g/cc | |
Michelman® VaporBase™ 1065 MVTR primer Description: MVTR primerUsage: VaporBase™ 1065 is a primer designed to be used in tandem with the VaporCoat® series of products. VaporBase™ 1065 works to seal the base substrate allowin.. |
|||
Specific Gravity | 1.27 - 1.29 g/cc | 1.27 - 1.29 g/cc | |
Michelman® VaporBase™ 1075 Water resistance primer Description: Water resistance primerUsage: VaporBase™ 1075 is a primer designed to be used in tandem with the VaporCoat® series of products as well as others. VaporBase™ 1075 works to s.. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina 40/447-FC-LMP Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina 601D10/1-A White PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina 602D02/101-C-AT-IS Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina 602D35/1-C-AT-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D 792 |
Karina 701D48/1-A-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina 760-35/1-IS-SD Ivory PVC Compound PVC compound for extrusion of monofilament.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D 792 |
Karina 800-25/1-IS Natural PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D 792 |
Karina 900D06/469-AT-IS Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina 95/222-D-AT-IS Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina E 18/548-RG-GE Gray Color Concentrate for PVC Color concentrate recommended for application in rigid PVC compounds for general purposes. Important Considerations:Heavy metal freeFormulated with organic and inorganic pigments PVC resin based (ca.. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 36/597-FC-LMP MB Concentration of Pigment Brown for PVC Heavy metal free pigment concentration for PVC usage. Minimum of 2%For rigid and flexible PVCInjection and extrusionExcellent for cables and wiresOrganic and inorganicInformation provided by Karina.. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina E 40/551-RG-GE Green Color Concentrate for PVC Color concentrate recommended for application in rigid PVC compounds for general purposes. Important Considerations:Heavy metal freeFormulated with organic and inorganic pigments PVC resin based (ca.. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina E 85/269-K-AT-IS-SI Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 6740 Moldings & Extrusions Flexible PVC Low gravity compound for extrusion and molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 8600 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, screen splines and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall EX1188A Wire & Cable Flexible PVC UL 360 jacket compound. 80°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 11890 Wire & Cable Flexible PVC High gloss, flame retardant jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 18753 Wire & Cable Flexible PVC Non-lead stabilized, fungus resistant 105 C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 1901 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 47551 Flexible PVC Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 873 Wire & Cable Flexible PVC 80°C rated, low migratory, oil resistant coil cord jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 8901 Moldings & Extrusions Flexible PVC Outdoor grade extrusion compound formulated for good UV light resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 48451 Moldings & Extrusions Flexible PVC Automotive window encapsulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |