Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.53 - 2.07 g/cc | 1.53 - 2.07 g/cc | |
Parker Chomerics Tecknit Teckfip™ FIP-E (SP)` Formed in Place Conductive Elastomer This is the small particle version of the Ag/glass (FIP E) compound that was specifically designed for the mobile cell phone applications. It should be noted that this compound offers a low compress.. |
|||
Specific Gravity | 1.53 - 2.07 g/cc | 1.53 - 2.07 g/cc | |
Parker Chomerics Tecknit Teckfip™ FIP-E Formed in Place Conductive Elastomer Commercial grade FIP compound designed for moderate shielding performance. The Ag/glass particles are very smooth which leads to very low compression set value. The material is also available as a h.. |
|||
Specific Gravity | 1.53 - 2.07 g/cc | 1.53 - 2.07 g/cc | |
Parker Chomerics Tecknit Teckfip™ HC FIP-E Formed in Place Conductive Elastomer Heat cure compound. Commercial grade FIP compound designed for moderate shielding performance. The Ag/glass particles are very smooth which leads to very low compression set value.Information provid.. |
|||
Specific Gravity | 2.03 - 2.07 g/cc | 2.03 - 2.07 g/cc | ASTM D792 |
Adamas Adalon® 113 PTFE, 23/2% Carbon/Graphite Filled Information provided by Adamas, HPM |