Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ISO 1183 |
S&E Specialty Polymers TufTech™ SE11-031 PVC Compound Application: Automotive - PVC, Integral Colored, Exterior Weatherable, Extrusion & Injection Molding CompoundInformation provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | NBR NM-IEC 60811-1-3 |
Karina 18/482-FC-LMP (SDB) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D 792 |
Karina 650D08/244-D-IS Beige PVC Compound Fungi resistant PVC compound, recommended for injection of bathroom carpet.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 830-48/1-IS-RG Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 835-42/14-IS-RG Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 846-32/64-IS-RG Orange PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 852-40/5-IS-RG Green PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 858-12/20-IS-RG PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 861-40/27-IS-RG Green PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 861-40/28-IS-RG Green PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 786-10/332-IS-RG Compound PVC White White rigid for spiral hoses (non-toxic)Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 80/274-IS-RG Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 80/321-IS-RG Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 806-21/10-IS-RG Coke PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 808-47/14-IS-RG Silver PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 811-40/312-IS-RG Green PVC Compound Non toxic PVC compound, recommended for blow molding of bottles for alcoholic beverages.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 836-10/132-IS-RG White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 898-02/160-IS-RG Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 835WA Wire & Cable Flexible PVC AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8642 Moldings & Extrusions Flexible PVC General purpose, fungus resistant extrusion and molding compound recommended for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 12860 Wire & Cable Flexible PVC 80C liquid tight conduit.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 16881 Coax & Telecom Flexible PVC 90C rated, non-lead stabilized jacket compound with excellent low temperature properties. Suitable for riser and optical fiber constructions.Information provided by Georgia GulfGeorgia Gulf became .. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 17940 Wire & Cable Flexible PVC THW insulation compound. Also suitable for 105C applications in 3/64 and larger sizes. UL recognized component for THW. Oil resistant I, VW-1 rated.Information provided by Georgia GulfGeorgia Gul.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 18901 Wire & Cable Flexible PVC General purpose, non-lead stabilized, 105°C rated jacketing compound. Formulated to have good migration resistance and flame retardant properties.Information provided by Georgia GulfGeorgia Gulf b.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 19930 Wire & Cable Flexible PVC THHN-THWN circuit sizes. Best suited for 105°C; 1/64 (18 AWG and larger). Rated VW-1. CSA approved TWN75, TEW, AWM IA, FT1 constructions. UL recognized for TW, THW, THWN, THHN. Oil resistant I.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 22851 Coax & Telecom Flexible PVC Non-lead stabilized, flame retardant jacket compound. Best suited for CM, CMR applications over FR PVC. Maximum service temperature rating of 75°C. UL recognized for 720 hr sunlight resistance.I.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 22905 Coax & Telecom Flexible PVC Non-lead tray cable jacket for 75°C maximum service temperature.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 19853 Wire & Cable Flexible PVC Non-lead stabilized insulation compound recommended for 105°C applications 1/32 wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 48562 Moldings & Extrusions Flexible PVC Automotive window encapsulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8911 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound. UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |