Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.15 - 2.22 g/cc | 2.15 - 2.22 g/cc | |
Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||
Specific Gravity | 2.15 - 2.18 g/cc | 2.15 - 2.18 g/cc | ISO 12086 |
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
Shamrock Technologies Fluoro FR-150 Anti-dripping Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins (and to polymeric resins containing glass fiber) provides greatly increased resistance to surface wear and abrasi.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
Shamrock Technologies Fluoro T® 615 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
Shamrock Technologies MicroFLON® 1437 Thermoplastic Grade PTFE Additive Used in high temperature engineering plastics.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion... |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® Chemfilm® DF100 Fluoropolymer Cast Film Description: Used for Chemical Process, Electrical/Electronics, Medical, Protective/Decorative. Surface Treatments Available: Chemical Etching (1 or 2 sides). Information provided by Saint Gobain Pe.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® Chemfilm® DF110 Fluoropolymer Cast Film Description: Used for Chemical Process, Electrical/Electronics, Medical, Protective/Decorative.Information provided by Saint Gobain Performance Products. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® Chemfilm® MR Fluoropolymer Cast Film Description: Commonly used for Aerospace/Release Film ApplicationsInformation provided by Saint Gobain Performance Products. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1900 Heat Bondable PTFE Film Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.005" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.006" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.062" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.250" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
Saint-Gobain Norton® T-200 Mechanical Grade PTFE Sheet (0.015" thick) Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate release sheets, .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
Shamrock Technologies Fluoro T® 602 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
Shamrock Technologies Fluoro T® 603 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
Shamrock Technologies Fluoro T® 611 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | at 25°C |
Daikin NEOFLON AP-201SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Good fluidity, suited to making moldings of complex shapes, requiring high fluidity.Information provided by Daikin Industries. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | at 25°C |
Daikin NEOFLON AP-231SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
3M Dyneon™ FEP 6303Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6303Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
3M Dyneon™ PFA 6502 TAZ Perfluoroalkoxy Fluorothermoplastic Granules 3M™ Dyneon™ PFA 6502TAZ is a fluorothermoplastic resin for compression molding applications. PFA 6502TAZ has a wide processing window with excellent color stability when longer residence times or .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | |
3M Dyneon™ PFA 6502 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are a new series of ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low leve.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
3M Dyneon™ PFA 6505TZ Fluoroplastic Granules 3M™ Dyneon™ Fluoroplastic Granules PFA 6505TZ (a fully fluorinated copolymer of tetrafluoroethylene and perfluorovinylether) has exceptional temperature resistance, excellent electrical properties.. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
3M Dyneon™ FEP 6307Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6307Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | @ 23°C, Sintering Molding; ASTM D4894-98a |
3M Dyneon™ TF 1641 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesVery .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | @ 23°C, Sintering Molding; ASTM D4894-98a |
3M Dyneon™ TF 1645 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesUsed .. |
|||
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
3M Dyneon™ PFA 6503 B EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 B EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |