Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ASTM D792 |
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ASTM D792 |
Quadrant EPP Symalit® PVDF (ASTM Product Data Sheet) |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ASTM D792 |
Quantum PVDF Information provided by Quantum Advanced Engineering Plastics |
|||
Specific Gravity | 1.78 - 1.80 g/cc | 1.78 - 1.80 g/cc | ASTM D792 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ASTM D792 |
Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings,.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ISO 1183 |
GEHR Plastics PVDF Polyvinylidene Fluoride Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ISO 1183 |
GEHR Plastics PVDF-ELS Polyvinylidene Fluoride, Electrically Conductive Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan.. |
|||
Specific Gravity | 1.78 - 1.83 g/cc | 1.78 - 1.83 g/cc | |
Shandong Dongyue Shenzhou New Material Co DS2601 Fluoroelastomer Copolymer Gum Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulc.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | Woven Density |
Saint-Gobain Chemlam® 4 Value Industrial Laminate Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass rei.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | Woven Density |
Saint-Gobain Chemlam® XF-200 Fully Sintered PTFE Coated, Flexible, Non-porous Fluoropolymer Laminated Composite Description: Chemlam® is the trademark for the Chemfab® family of flexible, non-porous fluoropolymer laminated composites that combine the features of multi-layer fluoropolymer cast films with.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | |
Silberline Silvex® 620-25-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ASTM D-792 |
Saint-Gobain Norton® PVDF Fluoropolymer Film Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | |
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ASTM D792 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |
|||
Specific Gravity | 1.78 - 1.82 g/cc | 1.78 - 1.82 g/cc | ASTM D792 |
Adamas Lakinor® U PVDF Information provided by Adamas, HPM |
|||
Specific Gravity | 1.78 - 1.80 g/cc | 1.78 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ASTM D792 |
Asahi Glass Fluon® AH-2000 LM-ETFE, Non-Conductive Type, Fluororesin Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive ag.. |
|||
Specific Gravity | 1.78 g/cc | 1.78 g/cc | ASTM D-792 |
Glastic GLASGUARD Scuff and Bulkhead Liners GlasGuard Scuff and Bulkhead Liners serve as a method of protecting trailer walls from damage caused by forklift trucks and careless loading and unloading of freight. Manufactured of 1/4" thick fib.. |
|||
Specific Gravity | 1.78 - 1.80 g/cc | 1.78 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |