Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Polymer Resources NY66-M40-[color]-H Nylon 66, 40% Mineral Filled, Heat Stabilized Nylon 66, 40% Mineral Filled, Lubricated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | Method A; ASTM D792 |
LNP Emi-X® OC-1008 LEX Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Radio Frequency Shielding, Electromagnetic Shielding, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Greene Tweed Arlon® 1286 Polyketone, Carbon Filled Greene Tweed offers precision plastic components for a variety of demanding semiconductor applications. These components are made from a full range of high-performance plastic materials including A.. |
|||
Specific Gravity | 1.49 - 1.55 g/cc | 1.49 - 1.55 g/cc | ASTM D 792 |
Karina E 835-10/155-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.49 - 1.55 g/cc | 1.49 - 1.55 g/cc | ASTM D 792 |
Karina E 835-18/115-C-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp OC008A PPS - Branched LNP* Thermocomp* OC008A is a compound based on Branched Polyphenylene Sulfide containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4012 Concentrate Based in Polyethylene DescriptionPOLYBATCH® 4012 is a blur color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 4.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Trelleborg R608 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Asahi Glass Fluon® AD639 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Asahi Kasei Thermofil P6-30MI-0533 30% Mica Reinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Trelleborg S862 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Gardenia P80515PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80515PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | uncatalyzed |
ACC QSil 60 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section .. |