Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Polymax® Maxelast® P3825 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Polymax® Maxelast® P3870 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Polymax® Maxelast® P3877 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Polymax® Maxelast® P3967H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Polymax® Maxelast® P1935 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Polymax® Maxelast® P1940 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Polymax® Maxelast® P3946 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | 20/20°C |
LyondellBasell TPM Tripropylene glycol methyl ether Information provided by Lyondell. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM 792 |
Multibase Multi-Flex® A 8406 A Natural TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM 792 |
Multibase Multi-Flex® D 5302 ELF Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ H6240B High Density Polyethylene Blow Molding Key Characteristics:Good stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthGood appearanceOdorlessSafe for food contactGood printabilityRecommended App.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-102 BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Total HDPE 6420 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:Excellent moisture barrier propertiesLow gelsLow taste and odorHigh stiffnessGood processabilityGood compatibility with.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ISO 1183 |
Total HDPE HD 6221 High Density Polyethylene - Blow Molding HDPE HD 6221 is a high density polyethylene with very high stiffness and impact resistance. The low viscosity of this grade has been designed for the manufacture of thin walled containers for foods.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D1505 |
Chevron Phillips Marlex® 9519H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, homopolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt strength.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Teknor Apex Sinelec CCB6814 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Corrugated Sheet Forms: Pellets Processing Method: Injection Method; Sheet Extr.. |
|||
Specific Gravity | 0.962 - 0.968 g/cc @Temperature 25.0 °C |
0.962 - 0.968 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ 9P-N Di Nonyl Phthalate Linear phthalate esterInformation provided by PolyOne |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | |
Radici Radilene® R 70 IE 0 2060 C High Density Polyethylene Shore hardness: 61 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D1505 |
SCG Chemicals EL-Lene™ H6140B High Density Polyethylene Blow Molding Key Characteristics:Good processabilityHigh stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthExcellent appearanceOdorlessSafe for food contactGood pri.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D792 |
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con.. |
|||
Specific Gravity | 0.962 g/cc | 0.962 g/cc | ASTM D1505 |
Chevron Phillips Marlex® 9518H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, homopolymer is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt strengthAre durable and recycl.. |