Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ISO 1183 |
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ISO 1183 |
Polimeri Europa Greenflex® MH 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MH 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Items produced with Greenflex MH 40 show high elasticity and good mechanical properties.Main Applic.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D792 |
PolyOne Elastamax™ HTE 1105 Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ISO 1183 |
Polimeri Europa Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 50 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FD 50 exhibit good optical and sealing properties, high flexibility and toughnes.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ISO 1183 |
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ M10 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium .. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ M3804 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium wa.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ M90 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ M9001 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such a.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ISO 1183 |
Total MDPE 3802 Medium Density Polyethylene, Blow Molding MDPE 3802 is a medium density polyethylene with good resistance to impact and excellent Environmental Stress Crack Resistance. It has been specifically designed for the blow molding of flexible con.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ISO 1183 |
Total MDPE 3802 Medium Density Polyethylene, Cable MDPE 3802 is a natural medium density polyethylene particularly suited for colored cable sheathing applications and designed to meet the requirements for telecommunication and power cables (medium a.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ISO 1183 |
Total MDPE HT 514 Medium Density Polyethylene, Blown Film MDPE HT 514 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HT 514 is a semi-high molecular weight polyethylene giving excellent mechanic.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D792 |
Teknor Apex Sinpolene FRF2074 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D792 |
E-Polymers EFLEX® V1060 EPDM/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |
|||
Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D792 |
E-Polymers EFLEX® V1070 EPDM/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |