Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ISO 1183 |
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ISO 1183 |
Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding of flexible items. Items produced with Greenflex ML 40 show high elasticity and flexibility.Main Applications: Gr.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet) |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D1505 |
LG Chemical LUTENE CCO550BK PE Compound Description: LUTENE CC0550BK offer the following properties: high mechanical properties, good environmental stress cracking resistance, excellent wetherability and high speed extrusion to give a smo.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | |
Struktol V-SSE Processing Additive Fatty acid esterTypical Applications: STRUKTOL® V-SSE has both internal and external lubricant characteristics. It is used in calendering, extrusion and injection molding applications. It also ha.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ M3504DXP Octene (C8) Rotational Molding Resin Natural base resin available in powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tanks, spray t.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ M70 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cyc.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ M735 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cycle.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D1928 C/D 1505 |
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 mas.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LPA815 LPA 815EVA DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR .. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LPA815 LPA 815EVA DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR .. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ISO 1183 |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ISO 1183 |
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ISO 1183 |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ISO 1183 |
Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding Lumicene® mPE M 3581 UV is a second generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 3581 UV is intended for the manufacture of rotomolded items.Its spec.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ISO 1183 |
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding Lumicene® mPE M 3509 is a metallocene-based medium density polyethylene combining the features of conventional blow molding polyethylene with differentiated optical propertied such as gloss and co.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LPA815 LPA 815EVA DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR .. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Specific Gravity | 0.935 g/cc @Temperature 25.0 °C |
0.935 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-0225 Silicone Fluid Is chemically equivalent to DOW CORNING® 225 FLUID. This product is a clear, low viscosity polydimethylsiloxane polymer with unique alcohol solubility for use in antiperspirants / deodorant applica.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D792 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Specific Gravity | 0.935 g/cc | 0.935 g/cc | ASTM D1505 |
SCG Chemicals EL-Lene™ M50 Octene (C8) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tan.. |