Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® MP 31 Low Density Polyethylene - Injection Molding Riblene MP 31 is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 are characterized by a medium rigidity.Main Applications: Riblene MP 31 i.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® MP 31 R Low Density Polyethylene - Injection Molding Riblene MP 31 R is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 R are characterized by a medium rigidity.Main Applications: Riblene MP .. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® MR 30 Low Density Polyethylene - Injection Molding Riblene MR 30 is a high fluidity low density polyethylene resin (LDPE) characterized by a high flowability and a medium rigidity.Parts made with Riblene MR 30 are characterized by good mechanical an.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile .. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Specific Gravity | 0.924 - 0.928 g/cc | 0.924 - 0.928 g/cc | ASTM D1505 |
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical Properties Additives: Antiblocking agent, Slip AgentApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | 15.6°C; ASTM D4052 |
ExxonMobil 26M Mobilgear SHC Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions oft.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ISO 1183 |
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating LDPE LA 0304 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum.Information provided by Total Pe.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Specific Gravity | 0.924 g/cc | 0.924 g/cc | ASTM D792 |
Entec Hypel® PELD50/.924 LDPE Available in North America Features: Food Contact Acceptable and Low DensityAgency Ratings: FDA 21 CFR 176.170, Table 2, Cond. B; Cond. C; Cond. D; Cond. E; Cond. F; Cond. G; Cond. H; and FDA 21 CF.. |