Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ISO 1183 |
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH .. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505 |
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9205 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Lids of all sizes, hous.. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505 |
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific.. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ LD1630J Low Density Polyethylene Injection Molding Key Characteristics:Good flowability for multicavitiesGood toughness and flexibilityExcellent gloss and transparencyOdorlessSafe for food contactRecommended Applications:HousewaresSmall to large clo.. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 |
Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH118 is a Linear Low Density Polyethylene, copolymer of hexene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 |
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability.. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 |
Braskem LH118 Blown Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 |
Braskem LH118 Linear Low Density Polyethylene Blends for irrigation pipes.Information provided by Braskem. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 |
Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene Description: LH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability... |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 |
Braskem LH218 Linear Low Density Polyethylene Insulation for low and medium tension XLPE wires and cables.Information provided by Braskem. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 |
Braskem LL118 Linear Low Density Polyethylene Blends for irrigation pipes.Information provided by Braskem. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 |
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
Specific Gravity | 0.916 g/cc | 0.916 g/cc | ISO 1183 |
Polimeri Europa Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Stretch films manufactured with Clearflex H&T CLH 196 have.. |