Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products P601-01 Polypropylene Copolymer, Black Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 - 0.916 g/cc @Temperature 25.0 °C |
0.910 - 0.916 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ DOZ-E Di (2-ethylhexyl) Azelate Branched C8 azelate ester with antioxidantContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | |
Honeywell PMP Polymethylpentene Film
(discontinued **) PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | |
Mapal Plastics Maplon Type D Polypropylene Sheet Main advantages: High clarity and medium haze, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy to convertMain disadvantages: Low scr.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | |
Mapal Plastics Maplon Type S Polypropylene Sheet Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D2240 |
Kraton® G1650 M (SEBS) Linear Triblock Copolymer Description: Kraton G1650 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM 792 |
Multibase Multi-Flex® D 5500 TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Blow MoldingInformation provided by Multibase |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2264B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P700J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P840J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsRecommended Applications:Automotive, motorcycle and electrical appliance part.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex TEKBOND® 6700-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7400-40D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Specific Gravity | <= 0.910 g/cc | <= 0.910 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 15°C; ASTM D4052 |
ExxonMobil Mobil Vaculine 148 The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti.. |
|||
Specific Gravity | 0.910 - 0.920 g/cc | 0.910 - 0.920 g/cc | |
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed Product Description: Epolene C-26 is a maleic anhydride grafted polyethylene coupling agent for polyethylene (PE) composites. The polar functionality and molecular weight are optimized to provide ba.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-21 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-21 is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity m.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-21P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-21P is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity modifier.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
Total PPH 3270 Polypropylene Homopolymer, High Crystallinity, Low Melt Flow Film Grade Low Residuals TOTAL Polypropylene 3270 utilizes the TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock. 3.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Diamond Polymers Softflex® 6001 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 0.910 - 0.940 g/cc | 0.910 - 0.940 g/cc | ASTM D792 |
Buckeye Polymers BP FLEX D6017 T BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Processing Method: Injection Mold.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-11 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-11 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |