Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100V-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-15 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-22 CRSX Polyester BMC Premi-Glas® 2103-22 CR-SX is a 22% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-25 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-25 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Specific Gravity | 1.35 - 1.85 g/cc | 1.35 - 1.85 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1401 Conductive Elastomer High performance for non-corrosive environments; soft(45 Shore A) for low closure force where gasket geometry cannot be exploited; low tear strength; no fluid resistance. Molded and ExtrudedRoHS Com.. |
|||
Specific Gravity | 1.65 - 1.85 g/cc | 1.65 - 1.85 g/cc | ISO 1183 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Specific Gravity | 1.65 - 1.85 g/cc | 1.65 - 1.85 g/cc | ISO 1183 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-15 CRSX Polyester BMC Premi-Glas® 2103-15 CR-SX is a 15% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.80 - 1.85 g/cc | 1.80 - 1.85 g/cc | ASTM D792 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 1.80 - 1.85 g/cc | 1.80 - 1.85 g/cc | ASTM D792 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | ASTM D792 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers. |