Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.52 - 1.58 g/cc | 1.52 - 1.58 g/cc | ASTM D792 |
PTS PBT-20GFR 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC. |
|||
Specific Gravity | 0.980 - 1.58 g/cc | 0.980 - 1.58 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 0860 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Extruded onlyRoHS CompliantInformation provided by Chomerics |
|||
Specific Gravity | 1.52 - 1.58 g/cc | 1.52 - 1.58 g/cc | NBR NM-IEC 60811-1-3 |
Karina 70911-35/1-HY-AC Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.52 - 1.58 g/cc | 1.52 - 1.58 g/cc | ASTM D 792 |
Karina 813-35/1-DY-SN-ERYB Compound PVC Ivory Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.52 - 1.58 g/cc | 1.52 - 1.58 g/cc | ASTM D 792 |
Karina 837-10/119-E-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.52 - 1.58 g/cc | 1.52 - 1.58 g/cc | ASTM D 792 |
Karina 837-35/1-E-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.52 - 1.58 g/cc | 1.52 - 1.58 g/cc | ASTM D 792 |
Karina E 48/1-IE Black Color Concentrate MBU Carbon black concentrate recommended for application in polyolefins and polyolefinic and PVC compounds for general purposes. Recommended usage of 2% to 4%.Information provided by Karina Indústri.. |
|||
Specific Gravity | 1.54 - 1.58 g/cc | 1.54 - 1.58 g/cc | ASTM D-792 |
Axiall 2460F Plenum Flexible PVC Plenum-grade optical fiber jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.52 - 1.58 g/cc | 1.52 - 1.58 g/cc | ASTM D792 |
BLUESTAR PBT 403M-G20 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Specific Gravity | 1.54 - 1.58 g/cc | 1.54 - 1.58 g/cc | ASTM D-792 |
Axiall 02520 Plenum Flexible PVC Non-lead stabilized plenum grade jacket with good low temperature properties. Recommended for Category 5 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2.. |