Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina 837-35/1-E-ERYB Ivory PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 837-35/1-E-ERYB Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
ASTM D 792
ASTM Color -1.67 - 1.33
-1.67 - 1.33
Color A, ME 12
4.08 - 7.08
4.08 - 7.08
Color B, ME 12
85.96 - 88.96
85.96 - 88.96
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 29.4 MPa
>= 4270 psi
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Profiles
Users viewing this material also viewed the following: