Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.07 - 1.11 g/cc | 1.07 - 1.11 g/cc | |
LG Chemical CP-RS Polycarboxylic Copolymer Description: CP-RS is the main raw material for concrete admixture, which improves water reducing ability of high early strength concrete. CP-RS exhibits superior property of early strength developm.. |
|||
Specific Gravity | 1.09 - 1.11 g/cc | 1.09 - 1.11 g/cc | |
Michelman® CleanGrip® 111 Alumina based, nonskid coating Description: Water based frictionizing agentUsage: CleanGrip® 111 is an alumina based, nonskid coating designed to reduce the slipperiness of shipping containers by providing excellent slide angl.. |
|||
Specific Gravity | 1.07 - 1.11 g/cc | 1.07 - 1.11 g/cc | |
LG Chemical CP-WBM Polycarboxylic Copolymer Description: CP-WRM is the main raw material for concrete admixture, which improves water reducing abilities. CP-WRM was developed through our advanced synthetic technologies, imparting good compati.. |