Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.90 - 4.10 g/cc | 3.90 - 4.10 g/cc | |
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3) Description: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, fria.. |
|||
Specific Gravity | 3.90 g/cc | 3.90 g/cc | Mixed; TM R050-16 |
Resinlab® SEC1244 Silver Filled Epoxy Adhesive Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth.. |
|||
Specific Gravity | 3.90 - 3.98 g/cc | 3.90 - 3.98 g/cc | ASTM D792 |
Isoflon PTFE + 60% Bronze Polytetrafluoroethylene with 60% Bronze Properties:Excellent wear and compression resistance (low cold creep)Good thermal conductivityImproved coefficient of friction when combined with Mos² or graphiteApplications: Dynamic seals for .. |
|||
Specific Gravity | 3.90 g/cc | 3.90 g/cc | ASTM D792 |
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers |
|||
Specific Gravity | 3.90 g/cc | 3.90 g/cc | |
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina Parts fabricated to print. Excellent physical properties and corrosion resistance. For pump liners, nozzles, guides. Standard crucibles and bolts, nuts and washers from 4-40 to 1/4-20. |
|||
Specific Gravity | 3.90 g/cc | 3.90 g/cc | Mixed; TM R050-16 |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |
|||
Specific Gravity | 3.90 g/cc | 3.90 g/cc | Mixed; TM R050-16 |
Resinlab® SEC1233 Silver Filled Epoxy Adhesive Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit.. |