Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.60 g/cc | 2.60 g/cc | ASTM D792 |
P & P Technology Nickel Graphite Loaded EPDM Molding grade conductive EPDM elastomer loaded with nickel graphite filler. The material is dark grey in color and is specially compounded to give high EMC performance and excellent IP sealing.Infor.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Allenâ„¢ Kaolin Allen is an intermediate-grained kaolin suitable for use as a filler and pigment in a wide variety of industrial applications such as soft rubber, plastics, ceiling tile, adhesives and paper product.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Franklin™ R Kaolin Franklin R is an intermediate-grained Kaolin used as a filler is “soft†rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by .. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Kaolexâ„¢ SC Kaolin Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 70°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-d Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 60°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-d Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® 35 Kaolin Clay - Waterwashed Coarse kaolin, milled powder, with the lowest oil absorption, for extending without thickening.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Wood.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® 80 Kaolin Clay - Waterwashed KaMin® 80 is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appli.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® 90 Kaolin clay - Waterwashed KaMin® 90 is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90 is ideally suited for solvent and water-borne paint, ink and adhesive applicati.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® 95 Kaolin Clay - Waterwashed KaMin® 95 is a medium-brightness, kaolin clay filler for paints, adhesives and related industries. It has a neutral pH, is acid-resistant and environmentally friendly.Industry: Adhesives & Sealan.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® HG Kaolin Clay - Waterwashed KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Nucap® 100G Kaolin Clay - Surface Treated Cost effective, moderate brightness, mercapto silane treated clay for partial thermal black replacement.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, EP.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyplate® P Kaolin Clay - Delaminated Polyplate® P is a high brightness, delaminated clay intended for use in latex paints, water flexography inks, water-based adhesives or water-based systems where increased hiding, tinting strength.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® 70 Kaolin Clay - Calcined Calcined clays, such as Polyfil® 70, are brighter than most water-washed clays, offering excellent processing and limited reinforcement. They impart outstanding wet/dry electrical properties due .. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® DLX Kaolin Clay - Delaminated Polyfil DLX is a large particle size, very high aspect ratio, delaminated clay that reduces gas and vapor permeability. It is a type of water washed clay which is processed to have a high aspect rat.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® F Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water .. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® WC Kaolin Clay - Calcined Polyfil®WC clay is an organo-functional calcined kaolin clay used in Wire and Cable and other thermoplastic applications. It is designed to reduce water vapor transmission, yields excellent wet a.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline Dedusted Flake Series DF-3500 Aluminum Flake DF-3500 Dedusted Aluminum Flake is manufactured by incorporating a small amount of Teflonâ„¢ with an uncoated aluminum pigment, and then, through further processing, is provided in a dry, non-dus.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline Dedusted Flake Series DF-3622 Aluminum Flake DF-3622 Dedusted Aluminum Flake is manufactured by incorporating a small amount of Teflonâ„¢ with uncoated aluminum pigment, and then, through further processing, is provided in a dry, non-dustin.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline SilBerCote® PC 3101X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline SilBerCote® PC 8153X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | crude vermiculite |
Skamol Group Exfoliated/Loose Vermiculite Loose Vermiculite SKAMOL exfoliated vermiculite has the following characteristics: Max. service temperature: Up to 1200°C (2192°F)Good thermal insulating propertiesLow densityLow heat capacityAbsorbing and free.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | ASTM D792 |
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound Data provided by Clariant Masterbatches |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | ISO 1183 |
Ecomass® 705BI79 BaSO4 Filled ABS Nontoxic alternative to traditional materials, radiation shielding applications.Moderate Specific GravityBaSO4 Powder Filled ABSInformation provided by Technical Polymers |