Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.34 g/cc | 2.34 g/cc | ASTM D792 |
PolyOne Gravi-Tech™ GT6000-0023 Black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Specific Gravity | 2.34 g/cc | 2.34 g/cc | |
Premix Thermoplastics PRESEAL® TPE 5020 General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o.. |
|||
Specific Gravity | 2.34 g/cc | 2.34 g/cc | uncured |
Atom Adhesives AA-BOND 2123 Epoxy Adhesive AA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. AA-BON.. |