Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.17 g/cc | 2.17 g/cc | ASTM D4895 |
3M Dyneon™ TFX 2035 PTFE
(discontinued **) Typical Applications: Liners, extruded tape, thick wall tubing.Information provided by the Dyneon division of 3M. |
|||
Specific Gravity | 2.17 - 2.24 g/cc | 2.17 - 2.24 g/cc | ASTM D792 |
Isoflon PTFE + 3% MoS2 Polytetrafluoroethylene with 3% Molybdenum disulfide Properties:Low coefficient of friction (static)Good thermal conductivityImproved wear resistanceOften combined with glass and bronzeApplications: Specially used for non-lubricated seals with period.. |
|||
Specific Gravity | 2.17 - 2.23 g/cc | 2.17 - 2.23 g/cc | ASTM D 792 |
Karina 1000/2065-IE MBPEB White (DT) Color Concentrate Filled white color concentrate recommended for polyolefins applications.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 2.17 - 2.23 g/cc | 2.17 - 2.23 g/cc | ASTM D 792 |
Karina E 1000/3055-IE MBPEB White Color Concentrate TIO2+ mineral concentrate recommended for polyolefins application (films, packaging, bags, etc.).Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 2.17 g/cc | 2.17 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Specific Gravity | 2.17 g/cc | 2.17 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP) LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers. |
|||
Specific Gravity | 2.17 g/cc @Temperature 25.0 °C |
2.17 g/cc @Temperature 77.0 °F |
|
Dow Corning SE 4422 SILICONE RTV One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning |
|||
Specific Gravity | 2.17 g/cc | 2.17 g/cc | |
Asahi Glass Fluon® CD145 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |