Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.13 - 2.23 g/cc | 2.13 - 2.23 g/cc | ASTM D1457-18; ISO.1183 DN.53479 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Specific Gravity | 2.13 - 2.18 g/cc | 2.13 - 2.18 g/cc | ISO 1183 |
Isoflon Virgin PTFE Polytetrafluoroethylene Properties/Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityExcellent resistance to continuous service temperatures up to 260°C, and, for limited per.. |
|||
Specific Gravity | 2.13 g/cc | 2.13 g/cc | ASTM D297, 15 |
Seals Eastern Perflas® 9295 Perfluorinated Rubber Perfluoro rubber for high-temperature, aggressive chemical service. Perflas 9295® seals offer high temperature service and are resistant to aggressive chemicals. They are a thermally stable, pe.. |
|||
Specific Gravity | 2.13 - 2.16 g/cc | 2.13 - 2.16 g/cc | |
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in .. |
|||
Specific Gravity | 2.13 - 2.16 g/cc | 2.13 - 2.16 g/cc | |
Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles) Usage: The resin can be used as the general required electric source, which is suitable for making film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop, fillin.. |
|||
Specific Gravity | 2.13 g/cc | 2.13 g/cc | ASTM-D792 |
CoorsTek PolyGlyde™ 2000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON F-104 PTFE Fine Powder Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON F-205 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into .. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder 15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1040 PTFE 20% Glass Fiber Filled Molding Powder 20% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder 20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder 15% glass fiber and 5% MoS2 filled. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanical and electrical service (e.g. split-curled bearings.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder 15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder 25% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by .. |
|||
Specific Gravity | 2.13 g/cc | 2.13 g/cc | |
Epoxy Technology EPO-TEK® H31D-LV Epoxy Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Specific Gravity | 2.13 g/cc | 2.13 g/cc | |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Specific Gravity | 2.13 - 2.16 g/cc | 2.13 - 2.16 g/cc | |
Shandong Dongyue Polymer DF-101 PTFE Molding Powder (Medium Particle Size) Usage: Can be processed to film, sheet, rob, gasket, axletree and presintered material.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE shou.. |
|||
Specific Gravity | 2.13 g/cc | 2.13 g/cc | ASTM D4745 |
3M Dyneon™ CC132 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a 10% carbon filled PTFE.Information provided by Dyneon, A 3M Company |