Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
Oceanchem Group Brominated Epoxy Oligomers-1 (BEP-1) Molecular Formula: (C36H32Br8O6)nCas No.: 68928-70-1Application: BEP-1 is used in ABS/HIPS etc.Information Provided by Oceanchem Group |
|||
Specific Gravity | 1.80 - 1.95 g/cc | 1.80 - 1.95 g/cc | |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D 792 |
SABIC Innovative Plastics Enduran 7062X PBT+PET (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
Parker Chomerics CHO-FORM® 5515 Robotically Dispensed Gasketing Description: CHO-FORM® 5515 One-component, thermal cure silicone system, with Ni/Graphite filler. Minimum cure temperature is 100°C (212°F). A low-cost solution for EMI shielding, it is specially.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
Parker Chomerics CHO-SHIELD® 611 Part A Conductive Coating Comments: Variant of CHO-SHIELD 596Typical Applications:Protecting EMI flangesInformation provided by Chomerics |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ISO 1183 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Specific Gravity | 1.80 - 1.85 g/cc | 1.80 - 1.85 g/cc | ASTM D792 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 1.80 - 1.84 g/cc | 1.80 - 1.84 g/cc | |
Shandong Dongyue Shenzhou New Material Co DS2602 Fluoroelastomer Copolymer Gum Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulc.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
Silberline Sparkle Silver® Premier 182 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2FL24 ETFE LNP* THERMOCOMP* 2FL24 is a compound based on ETFE resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is Wear Resistant. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | Cured |
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | IEC 1212-2 8.1 |
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2145 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2145 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2176 Fluoroelastomer Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneAbility for fast cure cycles with excellent processing safetyMedium viscosityProcess targets: compression and transfer molding, .. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2182 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2182 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2230 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2230 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FE 5520 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5520 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FE 5641Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5641Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
Cheng Yu Plastic E2345 Flame Retardant PET, 45% Glass Fiber |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FE 5622Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5622Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | |
Parker Chomerics CHO-BOND 1035 Electrically Conductive Sealant Electrically conductive, one component RTV silicone which provides both environmental sealing and EMI/RFI shielding. This sealant, filled with silver-plated glass particles, contains no acetic acid,.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
Premix Premi-Glas® 7203-28 28% Glass Reinforced Polyester SMC