Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.75 - 2.25 g/cc | 1.75 - 2.25 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Specific Gravity | 1.75 - 2.25 g/cc | 1.75 - 2.25 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |
|||
Specific Gravity | 1.75 - 1.76 g/cc | 1.75 - 1.76 g/cc | ASTM D792 |
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong.. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | ASTM D792 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer LNP* LUBRICOMP* KFL36 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | |
Silberline Sparkle Silvex® 965-30-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Orange LL10257/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL10257/4 is an orange color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® LL10257/4 is he.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE DescriptionPOLYBATCH® 20232U is a yellow color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability .. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | |
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Specific Gravity | 1.75 - 1.95 g/cc | 1.75 - 1.95 g/cc | |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
BCC Products METAL-KAST BC 8010 Urethane Casting New BC8010 is a quick setting urethane reproduction plastic system that simulates many of the desirable characteristics of aluminum metal. A highly machineable tooling material that is now easier to.. |
|||
Specific Gravity | 1.75 - 1.77 g/cc | 1.75 - 1.77 g/cc | ASTM D792 |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Specific Gravity | 1.75 - 1.77 g/cc | 1.75 - 1.77 g/cc | ASTM D792 |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Specific Gravity | 1.75 - 1.95 g/cc | 1.75 - 1.95 g/cc | |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Specific Gravity | 1.75 - 1.76 g/cc | 1.75 - 1.76 g/cc | ASTM D792 |
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Hylar 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and .. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Orange LL10257/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL10257/4 is an orange color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® LL10257/4 is he.. |