Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
NYCOA 5033 HST 33% Glass-Fiber Reinforced, Heat Stabilized, Translucent Nylon 66 Resin NYCOA 5033 HST is a 33% glass fiber reinforced, heat stabilized, translucent Nylon 66 resin used for injection molding. It has been specifically formulated for see through storage tanks for automoti.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable 1725-xx13FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable JG513GO Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Stat-Tech™ X ST6600-0041 ES NHFR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
S&E Specialty Polymers TufTech™ GA-8705-03 Natural Gloss PVC Compound Application: 75°C lead free, RoHS compliant riser jacketing compound.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Ovation Polymers Opnyl OP66GF33 Nylon 66, 33% Glass Reinforced, Conditioned Nylon 66 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Network Polymers Nylon 66G33L Description: Black NylonInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ±0.02; ISO 1183 |
PolyOne Bergadur™ PB400 G10 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
2065D Polyurethane-based Biomedical Elastomer |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Edgetek® PK-20CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Ravago Manufacturing Americas Hylex® P1010G20FRMA Polycarbonate, 20% Glass Filled Polycarbonate, 20% Glass Filled, Flame RetardantInformation provided by Ravago. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Fiberfil® M-2271 NAT Nylon 6, 33% Glass Reinforced, post industrial, natural Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Silberline Sparkle Silver® 3199-AR Sparkle Silver® 3199-AR is a medium non-leafing aluminum pigment. Its controlled particle size range makes it suitable for both one and two coat automotive and industrial coatings. Good orientati.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Silberline Sparkle Silver® 3333-AR Sparkle Silver® 3333-AR is an acid resistant pigment developed for formulators requiring good face whiteness, with a fine appearance. Close packing and good distinctiveness of image (D.O.I.) make.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Teknor Apex APEX® 84129 Polyvinyl Chloride, Flexible Notes: 80°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Specific Gravity | 1.38 - 1.44 g/cc | 1.38 - 1.44 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Brown 1028 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 1028 is a brown color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® 60175U/4 is a treated pine color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV s.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® 60175U/4 is a treated pine color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV s.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
DuPont Performance Polymers VESPEL TP-8395 Polyimide DuPont Vespel TP-8395 parts are specified for high-temperature and high-wear applications. TP-8395 parts offer an excellent balance of mechanical and thermal properties for superior performance in a.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Diamond Polymers NYLON 66GF33 Black Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D-792 |
Axiall 7450 Rigid PVC, Extrusion Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical Res.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 12792 Wire & Cable Flexible PVC General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 1055 Wire & Cable Flexible PVC NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |