Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Multibase TPSiV™ 3340-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | Of cured material |
Resin Technology Group UV-422 Flexible, UV Curing Sealant UV 422 is a semi-flexible, UV curing adhesive that can be used in a wide variety of potting, sealing, tacking and bonding applications. High strength bonds are formed to PVC and polycarbonate substr.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | |
Momentive Performance Materials Siloprenâ„¢ LSR 2680FC High Productivity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® G Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | |
Taiwan PU Corporation UR70 Polyester Urethane Rubber UR70 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Specific Gravity | 1.15 g/cc @Temperature 22.8 °C |
1.15 g/cc @Temperature 73.0 °F |
ASTM D792 |
Spartech PP5230 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlornated flame retardant system. UL94 V-1 rated. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7345-9000 TPE Product Description: StarFlex P 7345-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided .. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Teknor Apex ELEXAR® EL 8623 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-75A/B Elastomer KEG2000-75 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | PVC (80)/CP80AS2(20) |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Specific Gravity | 1.15 g/cc @Temperature 25.0 °C |
1.15 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® 25160 SILICONE RUBBER 60 durometer, peroxide cured, general purpose silicone rubber compoundInformation provided by Dow Corning |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | at working temperature |
C.O.I.M. UREXTER® T 400 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | |
ATG s.r.l. PVMQ Silicone Rubber |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | Mixed; TM R050-16 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | Mixed; TM R050-16 |
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate .. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Chase Plastics CP Pryme® PCA300 General Purpose Polycarbonate/ABS Alloy (Utility Grade) Information provided by Chase Plastics. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Lubrizol Estane® T865A Thermoplastic Polyurethane Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation |