Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | >= 0.930 g/cc | >= 0.930 g/cc | ISO.1183 DN.53479 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ISO 2781 |
Kraton® Cariflex™ IR0401 SU Polyisoprene Rubber Latex Description: Cariflex IR0401 SU Latex is a water-based emulsion of an anionically polymerized polyisoprene with a high cis-1,4 content, high molecular weight and a high linearity. The emulsion also.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Specific Gravity | 0.930 - 0.940 g/cc | 0.930 - 0.940 g/cc | |
Inhance Fluoro-Seal INHANCE® HD-1035 HDPE Product Description: INHANCE HD-1000 Series Polyethylene Particles are surface-activated High Density Polyethylene (HDPE) in particle or powder form. Surface activation makes the particles easy to.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
Teknor Apex Tekbond® TB 1372A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7100-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate DescriptionPOLYBATCH® ABPP-05 Antiblock is an antiblock concentrate containing 5% synthetic silica based in homopolymer polypropylene. This masterbatch is designed to provide high clarity, low haz.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ AO-25 Antioxidant Masterbatch Based in LDPE DescriptionPOLYBATCH® AO-25 is a general purpose antioxidant masterbatch based in LDPE. ApplicationThis concentrate is designed for use in polyethylene film and molding applications for improving .. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ MAS-25 Concentrate Based In LDPE DescriptionPOLYBATCH® MAS-25 is an organic antislip concentrate based in LDPE. This masterbatch is designed for use in moderate to heavy gauge film and sheet applications where extreme antislip p.. |
|||
Specific Gravity | 0.930 - 0.960 g/cc | 0.930 - 0.960 g/cc | |
Westlake Epolene® E-14E Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: The Epolene E-14E is a low molecular weight, low density, oxidized polyethylene. The low molecular weight and low softening point contribute to the production of stable, low col.. |
|||
Specific Gravity | 0.930 - 0.960 g/cc | 0.930 - 0.960 g/cc | |
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: Epolene E-20 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness and low color. It has a low softening point and low viscosity, which give .. |
|||
Specific Gravity | 0.930 g/cc @Temperature 25.0 °C |
0.930 g/cc @Temperature 77.0 °F |
|
Dow Corning Z-6697 SILANE Tetraethoxysilane (TEOS, Si(OC2H5)4) - diluent for zinc-rich primers, additive for other coupling agents.Information provided by Dow Corning |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
ExxonMobil Exxon™ 2222 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product for is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
ExxonMobil Exxon™ 2244 Fast Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber bales.Information provided by ExxonMobil Chemical |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
ExxonMobil Exxon™ 2255 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene.The product form is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 and ISO 1183 |
ExxonMobil Santoprene® 121-70M350 Thermoplastic Vulcanizate - UV Resistant Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for gap filler applications requiring scratch.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8211-55M300 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Specific Gravity | >= 0.930 g/cc | >= 0.930 g/cc | ISO.1183 DN.53479 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8291-55PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
AlphaGary AlphaSeal™ 240-6CY Blue 7002 Polyolefin Thermoplastic Elastomer AlphaSeal™ 240-6CY Blue 7002 is recommended for liners for plastic caps for carbonated soft drinks. It is formulated for low taste and odor and exhibits good elastic recovery, abrasion resistance a.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D4025 |
Kraton® D1119 P (SIS) Linear Triblock Copolymer Description: Kraton D1119 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Elastocon TPE Technologies Elastocon® OF65 Thermoplastic Elastomer Elastocon® OF65 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a reduced coefficient of f.. |