Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00500 - 0.00700 cm/cm @Thickness 3.17 mm |
0.00500 - 0.00700 in/in @Thickness 0.125 in |
ASTM D955 |
Oxford Polymers PC 714-FR Series PC, Flame retardant Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial.. |
|||
Linear Mold Shrinkage, Flow | 0.00500 - 0.00700 cm/cm @Thickness 3.17 mm |
0.00500 - 0.00700 in/in @Thickness 0.125 in |
ASTM D955 |
Oxford Polymers PEI 1000 PEI Product Description: (Unreinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Colors AvailableInformation provided.. |
|||
Linear Mold Shrinkage, Flow | 0.00500 - 0.00700 cm/cm | 0.00500 - 0.00700 in/in | Injection and Compression; ISO 2577 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Linear Mold Shrinkage, Flow | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | Compression; ISO 2577 |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Linear Mold Shrinkage, Flow | 0.00500 - 0.00700 cm/cm @Thickness 3.17 mm |
0.00500 - 0.00700 in/in @Thickness 0.125 in |
ASTM D955 |
Oxford Polymers PC C20-000 Clear PC Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl.. |
|||
Linear Mold Shrinkage, Flow | 0.00500 - 0.00700 cm/cm @Thickness 3.17 mm |
0.00500 - 0.00700 in/in @Thickness 0.125 in |
ASTM D955 |
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive.. |
|||
Linear Mold Shrinkage, Flow | 0.00500 - 0.00700 cm/cm @Thickness 3.17 mm |
0.00500 - 0.00700 in/in @Thickness 0.125 in |
ASTM D955 |
Oxford Polymers PEI 1010 PEI Product Description: (Unreinforced), Polyetherimide injection molding grade, high flow Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: .. |
|||
Linear Mold Shrinkage, Flow | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | Compression; ISO 2577 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Linear Mold Shrinkage, Flow | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | Compression; ISO 2577 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |