Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0020 - 0.0028 cm/cm @Time 86400 sec |
0.0020 - 0.0028 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP LX08411 PEEK LNP* THERMOCOMP* LX08411 is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added feature of this material is: Opaque. |
|||
Linear Mold Shrinkage, Flow | 0.00080 - 0.0028 cm/cm @Time 86400 sec |
0.00080 - 0.0028 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0023 - 0.0028 cm/cm @Thickness 3.20 mm |
0.0023 - 0.0028 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This .. |