Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00020 - 0.00080 cm/cm @Thickness 3.18 mm |
0.00020 - 0.00080 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.00080 cm/cm @Time 86400 sec |
0.00060 - 0.00080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.00080 cm/cm @Time 86400 sec |
0.00060 - 0.00080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DEF42 PC LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00040 - 0.00080 cm/cm | 0.00040 - 0.00080 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC006 is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.00080 cm/cm @Time 86400 sec |
0.00060 - 0.00080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10 LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00040 - 0.00080 cm/cm | 0.00040 - 0.00080 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Stat-kon DE006P PC (Europe-Africa-Middle East) LNP* Stat-kon* DE006P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the .. |