Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.029 cm/cm | 0.029 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KL003E POM (Europe-Africa-Middle East) LNP* LUBRICOMP* KL003E is a compound based on Acetal Copolymer resin containing PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.029 - 0.034 cm/cm @Thickness 3.20 mm |
0.029 - 0.034 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Linear Mold Shrinkage, Flow | 0.029 - 0.034 cm/cm @Thickness 3.20 mm |
0.029 - 0.034 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Linear Mold Shrinkage, Flow | 0.029 - 0.034 cm/cm @Thickness 3.20 mm |
0.029 - 0.034 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |