Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® ST820 BK503 PBT
(Unverified Data**) Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 4.00 mm |
0.018 in/in @Thickness 0.157 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66
(Unverified Data**) Zytel® ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance, high productivity and laser markability.Information provided by DuPont |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE25-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE70-FN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE90-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE70-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PA6/6 FR 346 RD Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 NAT Availability: North AmericaForms: PelletsAppearance: Natural ColorTPCI# 8384101Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® POM CO TX10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%) and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 HS MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 9094101Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 4.00 mm |
0.018 - 0.022 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA D51 PA6, Injection Molded Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 4.00 mm |
0.018 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin 100TL is a high viscosity acetal homopolymer containing 1.5% Teflo.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, Conditioned Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1863-BK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | DIS 294-4 |
Wellman Wellamid® 22L-NBK1/WE-1434 Nylon 66, Engineering Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, Conditioned Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |