Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0100 - 0.0310 cm/cm | 0.0100 - 0.0310 in/in | Average value: 0.0146 cm/cm Grade Count:41 |
Overview of materials for PVC, Flexible Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0250 cm/cm | 0.0100 - 0.0250 in/in | Average value: 0.0175 cm/cm Grade Count:4 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0350 cm/cm | 0.0100 - 0.0350 in/in | Average value: 0.0255 cm/cm Grade Count:29 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0500 cm/cm | 0.0100 - 0.0500 in/in | Average value: 0.0200 cm/cm Grade Count:8 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0200 cm/cm | 0.0100 - 0.0200 in/in | Average value: 0.0143 cm/cm Grade Count:14 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0300 cm/cm | 0.0100 - 0.0300 in/in | Average value: 0.0221 cm/cm Grade Count:20 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0180 cm/cm | 0.0100 - 0.0180 in/in | Average value: 0.0120 cm/cm Grade Count:33 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0130 cm/cm @Temperature 150 - 150 °C |
0.0100 - 0.0130 in/in @Temperature 302 - 302 °F |
Average value: 0.0109 cm/cm Grade Count:17 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0130 cm/cm @Time 900 - 900 sec |
0.0100 - 0.0130 in/in @Time 0.250 - 0.250 hour |
Average value: 0.0109 cm/cm Grade Count:17 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0250 cm/cm | 0.0100 - 0.0250 in/in | Average value: 0.0159 cm/cm Grade Count:16 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0250 cm/cm | 0.0100 - 0.0250 in/in | Average value: 0.0173 cm/cm Grade Count:7 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0400 cm/cm | 0.0100 - 0.0400 in/in | Average value: 0.0346 cm/cm Grade Count:102 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0200 cm/cm | 0.0100 - 0.0200 in/in | Average value: 0.0146 cm/cm Grade Count:13 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |