Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm @Thickness 3.17 mm |
0.0015 - 0.0025 in/in @Thickness 0.125 in |
|
Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Dry Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200H-15 Polyester SMC Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0025 cm/cm | 0.0010 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0025 cm/cm | 0.0010 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0025 cm/cm | 0.0020 - 0.0025 in/in | ASTM D955 |
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0025 cm/cm | 0.0010 - 0.0025 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® 12-033
(discontinued **) PRE-ELEC 12-033 is a conductive thermoplastic compound based on a polyacetal copolymer with 30% carbon fiber. PRE-ELEC 12-033 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | ASTM D955 |
PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | Injection Molding; ISO 2577 |
Vyncolit X658 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC 1050 Thermoset Polyester BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0025 cm/cm @Thickness 3.17 mm |
0.0020 - 0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ MP-15MCF/15T-2S Modified PPO - 15% Milled Carbon Fiber - 15% PTFE - 2% Silicone
(disconti Data provided by PolyOne. |