Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0041 cm/cm | 0.0041 in/in | ASTM D955 |
PolyOne Therma-Tech™ NJC-8500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0041 cm/cm | 0.0041 in/in | ASTM D955 |
Plenco 2567 Phenolic, Granular, Compression Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
Linear Mold Shrinkage | 0.0041 cm/cm | 0.0041 in/in | ISO 2577 |
Vyncolit A2710 Glass Fiber Reinforced Novolac Phenolic Vyncolit A2710 is a glass fiber reinforced phenolic molding compound with excellent mechanical and thermal properties.Information provided by Sumitomo Bak North America, Inc. |
|||
Linear Mold Shrinkage | 0.0041 - 0.0053 cm/cm | 0.0041 - 0.0053 in/in | Annealed; ASTM D955 |
Dow TF0807 TPO Dow Fascia TPO for Painted ApplicationsInformation provided by Dow |