Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00400 - 0.00700 cm/cm
0.00400 - 0.00700 in/in
ASTM D955
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00400 cm/cm
0.00400 in/in
ASTM D955
Niche Polymer PPCG40BK Copolymer PP, 40% Glass Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00400 - 0.0150 cm/cm
0.00400 - 0.0150 in/in
Average value: 0.00667 cm/cm Grade Count:6
Overview of materials for PEN-PET
This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent..
Linear Mold Shrinkage 0.00400 cm/cm
0.00400 in/in
Average value: 0.00400 cm/cm Grade Count:5
Overview of materials for Polycarbonate/Styrenic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage 0.00400 - 0.0110 cm/cm
0.00400 - 0.0110 in/in
Average value: 0.00760 cm/cm Grade Count:10
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron AN450M Flame Retardant ABS
Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade
High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron IMC25 ABS-PC Alloy
Medium FlowInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron SE45I Extrusion ABS
Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron TIM 200 MMA- ABS
High Impact(Transparent ABS)Information provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron TIM 300 MMA- ABS
High Impact(Transparent ABS)Information provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00500 cm/cm
0.00400 - 0.00500 in/in
ASTM D955
Bhansali Engineering Santron IMS 2000 SAN Resin
Clear SANInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron AN450M Flame Retardant ABS
Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00500 cm/cm
0.00400 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron HR60N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron SE32H Extrusion ABS
Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00500 cm/cm
0.00400 - 0.00500 in/in
ASTM D955
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin
High Transparent SANInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.0200 cm/cm
0.00400 - 0.0200 in/in
Average value: 0.0133 cm/cm Grade Count:29
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Linear Mold Shrinkage 0.00400 - 0.0140 cm/cm
0.00400 - 0.0140 in/in
Average value: 0.00857 cm/cm Grade Count:6
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.00400 - 0.0180 cm/cm
0.00400 - 0.0180 in/in
Average value: 0.0126 cm/cm Grade Count:4
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage 0.00400 - 0.0252 cm/cm
0.00400 - 0.0252 in/in
Average value: 0.0158 cm/cm Grade Count:51
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Linear Mold Shrinkage 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00580 cm/cm Grade Count:5
Overview of materials for Polypropylene with Glass Fiber + PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.00400 - 0.0130 cm/cm
0.00400 - 0.0130 in/in
Average value: 0.00719 cm/cm Grade Count:24
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade
Electroplating, High FlowInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron BL60 Impact modifier for PVC
Impact modifier for PVC, White powderInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade
Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00500 cm/cm
0.00400 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade
Super High Gloss, Medium ImpactInformation provided by Bhansali
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Bhansali Engineering Abstron IMC25 ABS-PC Alloy
Medium FlowInformation provided by Bhansali