Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 9.00e+6 g/mol | 9.00e+6 g/mol | |
Murtfeldt Material ”S”® 8000 Polyethylene Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding.. |
|||
Molecular Weight | 9.00e+6 g/mol | 9.00e+6 g/mol | |
Murtfeldt Original Material ”S”® plus + FP Polyethylene Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “.. |
|||
Molecular Weight | 9.00e+6 g/mol | 9.00e+6 g/mol | |
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from .. |
|||
Molecular Weight | 9.00e+6 g/mol | 9.00e+6 g/mol | |
Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive This material is electrically conductive and has half the sliding friction coefficient of the Original Material ”S”® enabling voltage to be dissipated at maximum speed with the same maximum frict.. |
|||
Molecular Weight | 9.00e+6 g/mol | 9.00e+6 g/mol | |
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan.. |
|||
Molecular Weight | 9.00e+6 g/mol | 9.00e+6 g/mol | |
Murtfeldt Original Material ”S”® plus + TLS Polyethylene Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i.. |