Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 50 - 60 m²/g | 50 - 60 m²/g | |
Zircar Zirconia ZYP-55 Zirconia Powder Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-55 has a surface area of 50.. |
|||
Specific Surface Area | 50 - 60 m²/g | 50 - 60 m²/g | |
Zircar Zirconia ZYP-55 Zirconia Powder Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-55 has a surface area of 50.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Calcium Carbonate Nanoparticles General DescriptionCalcium Carbonate (CaCO3) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Carbonate Particles are typically 10 - 80 nanometers (.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Dysprosium Nanoparticles General DescriptionDysprosium (Dy) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 10 - 80 nanometers (nm) with sp.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Dysprosium Oxide Nanopowder General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 -.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Erbium Nanoparticles General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Holmium Nanoparticles General DescriptionHolmium (Ho) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 30 - 80 nanometers (nm) with speci.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Niobium Nanoparticles General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Tantalum Nanoparticles General DescriptionTantalum (Ta) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tantalum Particles are typically 10-20 nanometers (nm) wi.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Terbium Nanoparticles General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Thulium Nanoparticles General DescriptionThulium (Tm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Thulium Particles are typically 25 - 100 nanometers (nm) with specifi.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Tin Nanoparticles General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Ytterbium Nanoparticles General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Calcium Phosphate Nanoparticles General DescriptionCalcium Phosphate (CAP) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Phosphate Particles are typically 10 - 80 nanometers (nm.. |