Polymer Property : Specific Surface Area = 30 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Calcium Carbonate Nanoparticles
General DescriptionCalcium Carbonate (CaCO3) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Carbonate Particles are typically 10 - 80 nanometers (..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Dysprosium Nanoparticles
General DescriptionDysprosium (Dy) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 10 - 80 nanometers (nm) with sp..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Dysprosium Oxide Nanopowder
General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 -..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Erbium Nanoparticles
General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Gadolinium Nanoparticles
General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with sp..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Holmium Nanoparticles
General DescriptionHolmium (Ho) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 30 - 80 nanometers (nm) with speci..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Indium Nanoparticles
General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Iron Nanoparticles
General DescriptionIron (Fe) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Iron Particles are typically 20-40 nanometers (..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Iron Nickel Nanopowder
General DescriptionIron Nickel ( FeNi) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nano..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Iron Oxide Nanopowder
General DescriptionIron Oxide ( Fe2O3 and Fe3O4) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure part..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Lithium Manganese Dioxide Nanoparticles
General DescriptionLithium Manganese Oxide (LiMnO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Manganese Oxide Particles are typically 10 - 50 na..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Lithium Nanoparticles
General DescriptionLithium (Li) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lithium Particles are typically 10 - 50 nanometers (nm) with specific..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Manganese Nanoparticles
General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Neodymium Nanoparticles
General DescriptionNeodymium (Nd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Neodymium Particles are typically 10 - 45 nanometers (nm) with spec..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Nickel Nanoparticles
General DescriptionNickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific s..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Nickel Titanium Nanoparticles
General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Niobium Nanoparticles
General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Samarium Nanoparticles
General DescriptionSamarium (Sm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Samarium Particles are typically 10 - 50 nanometers (nm) with specif..
Specific Surface Area 30 - 70 m²/g
30 - 70 m²/g
American Elements Silicon Nanoparticles
General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific su..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Strontium Carbonate Nanoparticles
General DescriptionStrontium Carbonate (SrCO3) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Strontium Carbonate Particles are typically 5 - 40 nan..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Tantalum Nanoparticles
General DescriptionTantalum (Ta) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tantalum Particles are typically 10-20 nanometers (nm) wi..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Terbium Nanoparticles
General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Ytterbium Nanoparticles
General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Yttrium Nanoparticles
General DescriptionYttrium (Y) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Yttrium Particles are typically 5 - 45 nanometers (nm) with specific s..
Specific Surface Area 30 - 80 m²/g
30 - 80 m²/g
American Elements Zirconium Nanoparticles
General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with ..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Calcium Phosphate Nanoparticles
General DescriptionCalcium Phosphate (CAP) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Phosphate Particles are typically 10 - 80 nanometers (nm..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Carbon Nanoparticles
General DescriptionCarbon (C) Nanoparticles, nanodots or nanopowder are black spherical high surface area graphitic carbon. Nanoscale Carbon Particles are typically 10 - 45 nanometers (nm) with spec..
Specific Surface Area 30 - 70 m²/g
30 - 70 m²/g
American Elements Copper Nanoparticles
General DescriptionCopper (Cu) Nanoparticles, nanodots or Nanopowder are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with ..
Specific Surface Area >= 30 m²/g
>= 30 m²/g
BET
Oceanchem Group Magnesium Hydroxide
Molecular Formula: Mg(OH)2Cas No.: 1309-42-8Use: Magnesium hydroxide is a non-halogen flame retardant recommended where use of halogenated products is limited or prohibited. In addition, it is an e..
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
American Elements Cobalt Iron Nanopowder
General DescriptionCobalt Iron ( CoFe) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties..