Physical Properties Metric English Comments
Particle Size 5.0 - 100 µm
5.0 - 100 µm
range
Potters Industries Q-Cel® 6048
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Particle Size 5.0 - 100 µm
5.0 - 100 µm
Potters Industries Q-Cel® 7040S Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Particle Size 70 - 100 µm
70 - 100 µm
Mean
Potters Industries Spheriglass® 2429 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Particle Size 4.00 - 100 µm
4.00 - 100 µm
Average value: 50.3 µm Grade Count:20
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Particle Size 80 - 100 µm
80 - 100 µm
Lucite International Colacryl ® DP300 Specialty Acrylic Resin
This is a high molecular weight PMMA resin. PMMA resins are characterised by high physical strength and abrasion resistance.Applications:This resin is used in the production of porous polymer molds ..
Particle Size 80 - 100 µm
80 - 100 µm
Lucite International Colacryl ® DP300S Acrylic Dental Resin
Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties...
Particle Size 80 - 100 µm
80 - 100 µm
Lucite International Colacryl ® DP300S Specialty Acrylic Resin
Colacryl® DP 300S has been designed for use as a dental polymer. Typical applications for this product include formulated, acrylic tooth polymer for manufacture of artificial teeth and denture ba..
Particle Size 75 - 100 µm
75 - 100 µm
Lucite International Colacryl ® DP300U Specialty Acrylic Resin
Colacryl® DP 300U has been designed for use as a dental polymer. Typical applications for this product include formulated, acrylic tooth polymer for manufacture of artificial teeth and denture ba..
Particle Size 72 - 100 µm
72 - 100 µm
Lucite International Colacryl ® PD12 Acrylic Dental Resin
Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties...
Particle Size 75 - 100 µm
75 - 100 µm
Lucite International Lucite® 1192 Glass Separation Resin
Lucite® 1192 is an ultra-high molecular weight PMMA resin, aimed at the protection of hard (metal oxide) coated glass sheets during storage and transportationLucite® 1192 acrylic resin provide..
Particle Size 95 - 100 µm
95 - 100 µm
RP-0886
Solvay AG-RHOâ„¢ DEP-775 Surfactant
Description: Anti-drift agent as adjuvants or to formulate into plant protection productsIdentification: DERIVATIZED NATURAL POLYMER CAS: 497-19-8 Water Solubility: Quick hydrationAvailable in: Asia..
Particle Size 90 - 100 µm
90 - 100 µm
150 mesh; PS-1-2
Solvay JAGUAR® HP 105 Surfactant
Description: Clear grade with excellent wet combing and detangling benefits. Recommended for use in a broad range of conditioning shampoos.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: H..
Particle Size 95 - 100 µm
95 - 100 µm
150 Mesh; PS-1-2
Solvay JAGUAR® 413 Surfactant
Description: Nonyl phenol based non ionic surfactant (70 EO)Chemical Name: GALACTOMANNAN BLENDCAS: 39421-75-5; 7631-86-9 Available in: Asia Pacific, Europe, Latin America and North AmericaApplicatio..
Particle Size 25 - 100 µm
25 - 100 µm
Laser diffraction; 90% range; ISO 13320
CRP Technology Windform® PS Polystyrene for Selective Laser Sintering
Windform® PS is a polystyrene based material, developed specifically to produce complex investment casting patterns. The sintered patterns are ideal for conventional wax infiltration, and become ea..
Particle Size 35 - 100 µm
35 - 100 µm
D10-D90
ALM PA 605-A Filled Nylon 12 Prototyping Polymer
50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a..
Particle Size 35 - 100 µm
35 - 100 µm
D10-D90
ALM PA-616-GS Filled Nylon 12 Prototyping Polymer
50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.The PA 616-GS can be processed on any laser..
Particle Size 35 - 100 µm
35 - 100 µm
D10-D90
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer
This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire..
Particle Size 35 - 100 µm
35 - 100 µm
D10-D90
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer
Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized..
Particle Size 30 - 100 µm
30 - 100 µm
D10-D90
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer
Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe..
Particle Size 35 - 100 µm
35 - 100 µm
D10-D90
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer
40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially ..
Particle Size 30 - 100 µm
30 - 100 µm
Range (D10 to D90); Laser Diffraction
ALM PA 620-MF Mineral Fiber Filled Nylon 12 SLS Prototyping Polymer
Information provided by Advanced Laser Materials (ALM).
Particle Size 30 - 100 µm
30 - 100 µm
Range (D10 to D90); Laser Diffraction
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines..
Particle Size 35 - 100 µm
35 - 100 µm
D10-D90
ALM PA-615-GS Filled Nylon 12 Prototyping Polymer
50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially ..